Surfiber PLC Splitter end face requirement
The connector end face grade can be divided into A zone, B zone and C zone according to the degree of importance, and the 400X end face detector is used for detection.
Area | Defect classification | Judgments based | Judgments |
Area A (within 25um)
| No defects are allowed | No defects | Failed |
Area B (25~120um) | scratch thickness | Width≤2um;≤3um 3pcs | Pass |
Width>3um | Failed |
scratch | have any black scratches | Failed |
Little point | Defect diameter>3 um | Failed |
width≤2um;≤3um 3pcs | Pass |
Area C (120-130um) | white scratch | width≤2um;≤5um 3pcs | Pass |
Little point | width≤2um ≤5um 3pcs | Pass |
Area D(130~250um) | defect | Can be wiped off the dirt | Failed |
Defect diameter≤10um | Pass |
Defect diameter>10um | Failed |
Remark:
1. The core is not allowed to have missing pieces and cracks.
2. Black scratches are not allowed in all areas of the end face.
3. The end face must be completely polished, and no cross scratches are allowed.
4. The end face is magnified 400 times, and no wipeable dirt is allowed in the 0-250um area.
5. According to the degree of importance, the connector end face grade can be divided into A, B, C and D, as follows: